MATERIALSTATIC COEF. (U)DYNAMIC COEF. (U)T FADING (ºC)WEAR RATE (mm3KWH)COMPRESSIVE STRENGTH (MPa)DATA SHEET
CR-2M0.40±0.05 μ0.45±0.05>350 °C20 (at 150 ºC)126±5 N/mm²HTML PDF
FAG18/150.45±0.05 μ0.52±0.05>450 °C30 (at 150 ºC)160±5 N/mm²HTML PDF
GHFM0.50±0.05 μ0.50±0.05>350 °C30 (at 150 ºC)190±5 N/mm²HTML PDF
SA80/050.60±0.05 μ0.57±0.05>350 °C80 (at 150 ºC)102±5 N/mm²HTML PDF
SA80/M0.60±0.05 μ0.50±0.05>340 °C60 (at 150 ºC)100±5 N/mm²HTML PDF
SF-BU0.43±0.05 μ0.35±0.05>400 °C30 (at 150 ºC)306±10 N/mm²HTML PDF
SF-MC20.45±0.05 μ0.40±0.05>400 °C30 (at 150 ºC)306±10 N/mm²HTML PDF
TOP/050.60±0.05 μ0.50±0.05>300 °C40 (at 150 ºC)143±5 N/mm²HTML PDF